EDF Finds Hints of Stress Corrosion Crack at Nuclear Reactor

Electricite de France SA found indications that “stress corrosion” cracks may again affect pipes at a nuclear reactor that it fixed fewer than three years ago, risking a revival of tensions on Europe’s power and gas markets.